← すべての投稿099 / SINTERLAB
2018Russian Journal of Inorganic Chemistry

ゾルゲル法により製造された HfB2-30 vol % SiC UHTC の表面に対する超音速解離空気流の影響

Иллюстрация к 出版物 «ゾルゲル法により製造された HfB2-30 vol % SiC UHTC の表面に対する超音速解離空気流の影響»099
SINTERLAB · RESEARCH IMAGE
作者

Simonenko, E.P., Simonenko, N.P., Gordeev, A.N., Kolesnikov, A.F., Papynov E.K., Shichalin, O.O., Tal’skikh, K.Y., Gridasova, E.A., Avramenko, V.A., Sevastyanov, V.G., Kuznetsov, N.T.

記事の内容

要約

099 / SINTERLAB

Abstract⎯A new method to produce ultra-high-temperature ceramic composites under rather mild conditions (1700°C, 30 MPa, treatment time 15 min) was applied to synthesize a relatively dense (ρrel = 84.5%) HfB2–30 vol % SiC material containing nanocrystalline silicon carbide (average crystallite size ~37 nm). The elemental and phase compositions, microstructure, and some mechanical properties of this material and also its thermal behavior in an air flow within the temperature range 20–1400°C were investigated. Using a highfrequency induction plasmatron, a study was made of the effect of a supersonic dissociated air flow on the surface of the produced ultra-high-temperature ceramic composite shaped as a flat-end cylindrical sample installed into a copper water-cooled holder. On 40-min exposure of the sample to the supersonic dissociated air flow, the sample did not fail, and the weight loss was 0.04%. Although the heat flux was high, the temperature on the surface did not exceed 1400–1590°C, which could be due to the heat transfer from the sample to the water-cooled model. The thickness of the oxidized layer under these conditions was 10–20 μm; no SiC-depleted region formed. Specific features of the microstructure of the oxidized surface layer of the sample were noted.